Experimental study on two-stage aging treatment of ZTM630 magnesium alloy

WANG Na-na1, ZHOU Ji-xue1, LIU Yu1, ZHAO Dong-qing1, MA Bai-chang1, YANG Yuan-sheng2   

  1. 1.Shandong Engineering Research Centre for Lightweight Automobiles Magnesium Alloy, Shandong Provincial Key Laboratory for High Strength Lightweight Metallic Materials, Advanced Materials Institute, Qilu University of Technology (Shandong Academy of Science), Jinan 250014, China; 2. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016,China
  • Received:2017-10-08 Online:2018-06-20 Published:2018-06-20

Abstract:

By changing the finalaging time, the microstructure evolution and mechanical properties of extruded Mg-6Zn-3Sn-0.5Mn alloy were investigated by means of optical electron microscopy, scanning electron microscopy and transmission electron microscopy. Results showed that through the twostep aging treatment, the suitable parameter was 90 ℃×12 h+180 ℃×8 h. Under this parameter, ultimate tensile strength and elongation of the alloy reached 383.1 MPa,7.667%, respectively. After two-step aging treatment, there were dispersed and fine precipitates precipitated in matrix and grain boundaries, which were mainly of Mg2Sn and MgZn2 phases. During the process of stretching, the precipitation strengthen effect of dispersed fine precipitated phase and the strengthening effect inhibiting the grain movement made the mechanical properties of the alloy better.

Key words: Mg-Zn-Sn-Mn alloy, two-step aging treatment, microstructure