J4 ›› 2010, Vol. 23 ›› Issue (6): 52-56.

• Content • Previous Articles     Next Articles

Impact Ductility of Rotating Arc Narrow Gap Horizontal GMAW Joint

 LUO Fei, GUO Ning, JIA Chuan-Bao, XUE Liang-Chang, CHENG Shuang-Qiu, ZHANG Lin-Lin   

  1. Shandong Provincial Key Laboratory of Ocean Environment Monitoring Technology, Institute of Oceanographic Instrumentation, Shandong Academy of Sciences, Qingdao 266001, China
  • Received:2010-08-31 Published:2010-12-20 Online:2010-12-20

Abstract:

         We developed a novel rotating arc horizontal wielding technology. Previous results indicated that this technology could effectively control the molten pool behavior of horizontal wielding, and eliminate the negative of wielding slit sinking. This paper further investigates the impact ductility of the novel rotating arc narrow gap horizontal GMAW joint of the 12Ni3CrMoV steel.Results demonstrate that the average impact energy of the base material, heat affected zone (HAZ) and wield zone is 236 J, 212.2 J and 115.4 J when temperature is 0℃. The impact ductility of HAZ only approximately decreases 10.2%, as compared with that of the base material. This shows that the thermal cycle of rotating arc narrow gap horizontal GMAW does not significantly deteriorate the ductility of the base material.

Key words: impact ductility, horizontal wielding, rotating arc

CLC Number: 

  • TG444+.3

Open Access This article is licensed under a Creative Commons Attribution-NonCommercial 4.0 International License (CC BY-NC 4.0), which permits third parties to freely share (i.e., copy and redistribute the material in any medium or format) and adapt (i.e., remix, transform, or build upon the material) the articles published in this journal, provided that appropriate credit is given, a link to the license is provided, and any changes made are indicated. The material may not be used for commercial purposes. For details of the CC BY-NC 4.0 license, please visit: https://creativecommons.org/licenses/by-nc/4.0